C4
|  |
 |
 |
 We have not this metal on permanent stock. But we can supply it with a longer delivery time, in any needed shape.
|
Carlier designation | ND16CT |
UNS designation | N06455 |
European numbering designation | 2.4610 |
AFNOR designation | NiMo16Cr16Ti |
Thyssen Krupp VDM designation | Nicrofer 6616HMo |
Applicable standards | ASTM B574 | Bars | ASTM B575 | Plates |
|
Chemical composition
en % | Ni | Mo | Fe | Cr | C | Co | Mn | S | Si | P | Ti | min | - | 14,000 | - | 14,000 | - | - | - | - | - | - | - | max | Solde | 17,000 | 3,000 | 18,000 | 0,015 | 2,000 | 1,000 | 0,030 | 0,080 | 0,040 | 0,700 |
Density : 8.89
Guarantee mechanical results in MPa
Standard | Rm | Rp 0.2% | A % | Z | HB | Hrc | Comments | ASTM B574 - 99a | 690 | 276 | 40 | - | - | - | All diameters | ASTM B575 - 99a | 640 | 276 | 40 | - | 100 | - | |
Forging conditions
Forging is made at a range of temperature included between 1150 and 950°C, then cooled at appropriate conditions for the final thermal treatment and obtain required characteristics. In any case, please contact us.
Properties / Main use conditions
"C" family alloy, Ni-Cr-Mo without W and with Co and Ti, appeared at the beginning of the 70, which presents a great metallurgical stability. Utilisation contitions are nearly the same as C276, but with a smaller resistance in reducing atmospheres and a higher resistance in oxidizing atmospheres.
Main applications
Production of fertilizers and pesticides. Production of acetic acid.
Heat treatment
Please, contact us
|