205
|  |
 |
 |
 We do not commercialize this metal
|
Carlier designation | 205 |
UNS designation | N02205 |
European numbering designation | 2.4061 |
AFNOR designation | LC-Ni 99.6 |
Thyssen Krupp VDM designation | LC-Nickel 99.6 |
Applicable standards | ASTM F1 | Specific applications | ASTM F3 | Specific applications |
|
Chemical composition
en % | Ni | Cu | Fe | Mn | C | Mg | min | 99,600 | - | - | - | - | - | max | - | 0,100 | 0,200 | 0,300 | 0,020 | 0,050 |
Density : 8.89
Forging conditions
Forging is made at a range of temperature included between 1150 and 950°C, then cooled at appropriate conditions for the final thermal treatment and obtain required characteristics. In any case, please contact us.
Properties / Main use conditions
Nickel with a low carbon percentage, and high purity (99,6% min.) ; it is sometimes used in the same conditions as 201, but more often for use with special physical properties, electrical resistivity.
Main applications
Food industry, powerfull electrical industry, unactive electronic components, semiconductor caps. Same properties as 200.
Heat treatment
Please, contact us
|